NC-39

Welding Electrode NC-39

PREMIARC

Welding Electrode NC-39, E309-16 is a high-quality welding electrode with calcium-titanium flux, ideal for welding a wide range of metals. Available for all welding positions with superior precision and crack resistance.

Classification

AWS A5.4 E309-16

Product Description

KOBE Steel NC-39 KOBELCO, E309-16 welding electrode is a multi-purpose welding electrode with calcium-titanium flux for welding ferritic steels and dissimilar metal joints.

Suitable for use on AC or DC-EP in all positions, producing high-quality welds with excellent crack resistance.

Product Specifications

ParametersDescription
Product NameWelding Electrode NC-39
BrandKOBELCO
Electrode TypeWelding Electrodes for Stainless Steel
Welding Electrode Size2.6 mm, 3.2 mm, 4.0 mm
Welding ProcessSMAW
Weight Per Packaging20 Kg
PolarityAC, DCEP
AWS StandardAWS A5.4 E309-16
Re-Drying Conditions150–200°C × 0.5–1 hour
Identification ColorFirst Color: Black, Second Color: White

Work Ability

  • KOBE Steel NC-39 is a welding electrode with calcium-titanium flux, providing structured welded joints.
  • NC-39 welding electrode is suitable for welding dissimilar metal joints and as a base for ferritic steel. This electrode can be used in both AC and DC-EP (positive) polarities for all welding positions.
  • Provides good weldability and superior crack resistance.

Welding Positions

posisi pengelasan kawat las nc-39

KOBELCO NC-39 electrodes can be used in various welding positions—including flat, horizontal, vertical-up, and overhead—offering stable arc characteristics and good weld pool control.

  • 1F (Flat Fillet)
  • 1G (Flat Groove)
  • 2F (Horizontal Fillet)
  • 2G (Horizontal Groove)
  • 3G Uphill (Vertical Up Groove)
  • 4G (Overhead Groove)

Welding Parameters (A)

Recommended welding current parameters for KOBELCO NC-39 electrodes, based on electrode diameter and welding position, to ensure a stable arc and optimal weld quality.

Diameter (φ mm)1F, 1G, 2F, 2G (A)3G Uphill, 4G (A)
2.050–7545–65
2.675–9570–90
3.285–12080–115
4.0110–16090–140
5.0150–200

Mechanical Properties of Welded Products

Mechanical properties of KOBELCO NC-39 weld metal based on typical test results (AC) and guaranteed minimum values ​​in accordance with standards.

ParametersTypical Value (AC)Collateral Value
0.2% Yield Strength (YS)410 MPa
Tensile Strength (TS)590 MPa≥ 552 MPa
Elongation (EL) on 4D39%≥ 30%
Impact Value (IV) at 0°C62 J

Chemical Composition of Weld Metal

Chemical composition of all welded metals (mass %)

ElementTypical Value (AC)Collateral Value
C (Carbon)0,07≤ 0,15
Si (Silikon)0,40≤ 1,00
Mn (Manganese)1,00,5–2,5
P (Phosphorus)0,03≤ 0,04
S (Sulfur)< 0,01≤ 0,03
Ni (Nickel)13,412,0–14,0
Cr (Chromium)23,922,0–25,0
Mo (Molybdenum)0,21≤ 0,75
Cu (Copper)0,12≤ 0,75

Note: Single values ​​represent the maximum permissible limits.

Packaging Data

Packaging information for KOBELCO NC-39 electrodes, based on diameter, electrode length, weight per package, total weight per carton, weight per rod, and carton dimensions.

Diameter (φ mm)Length (mm)kg/packkg/cartong/stickCarton Size (mm)
2.025022011300W × 125H × 280L
2.630022020300W × 100H × 330L
3.235052036175W × 115H × 380L
4.035052055175W × 115H × 380L
5.035052082175W × 115H × 380L

Shipping Approval

KOBELCO NC-39 electrodes have obtained approval from various international classification societies to ensure their quality and reliability in industrial applications.

CertificationCertification Code
ABSMG (AWS A5.4 E309-16)
LRSS/CMn m (Chem.)
DNVVL309, MG
BVUP (E309-16)
NKKD309
CCSAS2-B

Note: a) Testing uses AC (Alternating Current).

Notes of Usages

  • Re-dry the electrodes at a temperature of 150°C – 200°C for 30–60 minutes before use.
  • Keep the arc length shorter to create sufficient protection for the weld pool, thereby preventing porosity.
  • The width of the movement (weaving) must be 2.5 times smaller than the diameter of the electrode to obtain adequate protection.
  • Use the recommended welding parameters to prevent the electrode from burning due to Joule heating.
  • No preheating is required for welding stainless steel, but the interlayer temperature must be maintained at 150°C.

Want to order KOBELCO NC-39 Welding Electrode? Contact our team now.

ISO certificate

ISO 9001:2015

ISO 14001:2015

© 2026, PT. Intan Pertiwi Industri | All Rights Reserved.